Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.121 GPa | 17.5 ksi | ASTM D638 |
3M Dyneon™ CCX1029 PTFE, 10% Carbon Fiber Filled
(discontinued **) Type I, non-free-flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon .. |
|||
Tensile Modulus | 0.121 GPa | 17.5 ksi | ASTM D638 |
3M Dyneon™ CC503 PTFE, 15% Mineral Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings - FDA compliant, valve seats, seals.Data provided by Dyneon. |