Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.117 GPa | 17.0 ksi | |
Loctite® 3872 1 component acrylic/urethane UV/Heat Cure Flexible Adhesive Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or.. |
|||
Tensile Modulus | 0.117 GPa | 17.0 ksi | ISO 527-2/1A/1 |
ExxonMobil LDPE LD 650 Low Density Polyethylene Resin (European Grade) Product Description: LD 650 is an easy flowing LDPE grade with a good flexibility and excellent toughness.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No.. |