Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0880 GPa | 12.8 ksi | ISO 527 |
Lubrizol ESTANE® 58141 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |