Polymer Property : Tensile Modulus = 0.0510 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.0510 GPa
7.40 ksi
Molded Properties; ISO 527-2/1
ExxonMobil Escorene™ FL 00714 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00714 is an easy processable grade for extrusion coating, co-extrusion coating and cast film. This grade offers excellent heat sealing characteristics and excellent optical p..
Tensile Modulus 0.0510 GPa
7.40 ksi
1 mm/min
Arkema Group Pebax® MX 1059 Polyether Block Amide (PEBA) (Dry)
POLYETHER BLOCK AMIDE (PEBA) Hardness 35 shore D Good resistance to oils. Applications: Automotive, cable...ISO data provided by the manufacturer, Arkema.