Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.00689 GPa | 0.999 ksi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable JJF102L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Modulus | 0.00689 GPa | 0.999 ksi | Type IV, 510 mm/min; ASTM D638 |
PolyOne FireCon™ CPE 30-2 RoHS BLACK Polyethylene, Chlorinated (CPE) CPE-30-2 RoHS BLACK is a RoHS compliant heavy duty thermoplastic jacket for power and control cables. It is suitable for VW1 and tray fire rated applications. CPE-30-2 RoHS BLACK has a good balance .. |
|||
Tensile Modulus | 0.00689 GPa | 0.999 ksi | Type IV, 510 mm/min; ASTM D638 |
PolyOne FireCon™ CPE 32-33 RoHS Black Polyethylene, Chlorinated (CPE) CPE-37-11 RoHS BLACK is a heavy duty thermoplastic jacket for power and control cables. It is suitable for VW1 and tray fire rated applications. CPE-37-11 RoHS BLACK offers the highest physical prop.. |
|||
Tensile Modulus | 0.00689 GPa | 0.999 ksi | Type IV, 510 mm/min; ASTM D638 |
PolyOne FireCon™ CPE 37-11 RoHS BLACK Polyethylene, Chlorinated (CPE) CPE-37-11 RoHS BLACK is a heavy duty thermoplastic jacket for power and control cables. It is suitable for VW1 and tray fire rated applications. CPE-37-11 RoHS BLACK offers the highest physical prop.. |
|||
Tensile Modulus | 0.00689 GPa | 1.00 ksi | Storage |
Epoxy Technology EPO-TEK® OG133-8 UV Cure Optical Epoxy Material Description: A single component, UV curable, thixotropic flexible epoxy adhesive/encapsulant designed for semiconductor and opto-electronic packaging. Glob top over IC and wire bonds, and .. |