Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.00294 GPa | 0.426 ksi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3715 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |