Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.000345 GPa | 0.0500 ksi | ASTM D3574 |
Saint-Gobain Korel® K30-15 Soft Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi.. |
|||
Tensile Modulus | 0.000345 GPa | 0.0500 ksi | ASTM D3574 |
Saint-Gobain Korel® K40-30 Medium Deflection Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi.. |
|||
Tensile Modulus | 0.000345 GPa | 0.0500 ksi | ASTM D3574 |
Saint-Gobain Korel® K40-35 Medium Deflection Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc.. |