Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K Factor (ISO) | 2.9 µm/km @Temperature 240 °C |
2.9 µm/km @Temperature 464 °F |
|
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol.. |