Mechanical Properties Metric English Comments
K Factor (ISO) 2.7 µm/km

@Temperature 100 °C
2.7 µm/km

@Temperature 212 °F
Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy
Main Characteristics: Modified friction wear; Tough; Soft; Reduced wear at temperatures at 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInfor..