Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K Factor (ISO) | 1.5 µm/km @Temperature 200 °C |
1.5 µm/km @Temperature 392 °F |
|
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn.. |
|||
K Factor (ISO) | 1.5 µm/km @Temperature 20.0 °C |
1.5 µm/km @Temperature 68.0 °F |
|
Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy Main Characteristics: Hard; Stiff; Tough; High dimensional stability; High fatigue strength; High weather resistance; Good fire behavior; Suitable for vacuum; Good machinability; Contains PTFE; Stre.. |