Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K Factor (ISO) | 1.1 µm/km @Temperature 20.0 °C |
1.1 µm/km @Temperature 68.0 °F |
|
Wolf Kunststoff ZEDEX® ZX-100MT A1T Polymer Alloy, Mineral Reinforced Stiff; Hard; Very high strength; No fiber reinforcementApplications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automotive Technology, Machine ToolsInformation provided by Zed.. |
|||
K Factor (ISO) | 1.1 µm/km @Temperature 100 °C |
1.1 µm/km @Temperature 212 °F |
|
Wolf Kunststoff ZEDEX® ZX-530 A5D Polymer Alloy Main Characteristics: Low Creep; Low moisture absorption; Flame retardant; Low impurity ions; Good machinability; FDA compliant LABS; Extremely low outgassing; Less expensive than PEEK; Stress resis.. |