Polymer Property : K Factor (ISO) = 0.80 µm/km Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K Factor (ISO) 0.80 µm/km

@Temperature 200 °C
0.80 µm/km

@Temperature 392 °F
Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy
Main Characteristics: Modified friction wear; Tough; Soft; Reduced wear at temperatures at 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInfor..