Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K Factor (ISO) | 0.20 µm/km @Temperature 20.0 °C |
0.20 µm/km @Temperature 68.0 °F |
|
Wolf Kunststoff ZEDEX® ZX-410V7T A4T Polymer Alloy, Fiber Reinforced, Friction Modified Main Characteristics: Fiber-reinforced; Friction-modified; Very high stiffness (higher than that of fiber-reinforced PEEK); Very low thermal expansion coefficient; Low friction; High wear resistance.. |
|||
K Factor (ISO) | 0.20 µm/km @Temperature 100 °C |
0.20 µm/km @Temperature 212 °F |
|
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn.. |