Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Resistance | 4800 N @Temperature 23.0 °C |
1080 lb (f) @Temperature 73.4 °F |
ISO 6603-2 |
Covestro Makrolon® 6165 X Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Low.. |