Mechanical Properties Metric English Comments
Tensile Strength, Yield 995 MPa

@Strain 0.200 %
144000 psi

@Strain 0.200 %
Haynes 556® alloy, 30% cold reduction
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Tensile Strength, Yield 995 MPa

@Strain 0.200 %,
Temperature 540 °C
144000 psi

@Strain 0.200 %,
Temperature 1000 °F
Haynes 718 alloy, cold rolled, solution-treated and aged sheet
Cb and Ta content combined weight percentage of 5. Excellent high-temperature strength up to 650°C, good ductility, formability, and weldability. Very good welding characteristics. Applications i..