Tensile Strength, Yield 670 MPa

@Strain 0.200 %,
Temperature 760 °C
97200 psi

@Strain 0.200 %,
Temperature 1400 °F
Haynes 25 alloy, cold worked sheet, 20% cold reduction, aged at 370°C (700°F) for 1 hour
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Yield 670 MPa

@Strain 0.200 %
97200 psi

@Strain 0.200 %
Haynes 625 alloy, plate after 8000 hours at 760°C (1400°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Tensile Strength, Yield 670 MPa
97200 psi
Universal Wire Works E91T1-B3 Flux Cored Carbon Steel Tubular Electrode
Alloy 91T1-B3 is a low alloy steel electrode for single and multiple pass welding of 2.25% chromium, 1 % molybdenum high temperature creep resistant steels in all positions. The fast freezing slag s..
Tensile Strength, Yield 670 MPa

@Temperature 75.0 °C
97200 psi

@Temperature 167 °F
Wet; EN2561
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber
Information provided by HexCel
Tensile Strength, Yield <= 670 MPa

@Strain 0.200 %
<= 97200 psi

@Strain 0.200 %
CLAL-MSX ARCAP Anticorrosion AP4 H15 Spring, Rolled Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Tensile Strength, Yield 670 MPa
97200 psi
R<sub>p</sub>0.2, @RT, 270 HB.
Assab Steels CARMO Cold Work Steel
CARMO is a high-strength, flame-induction and through hardening steel delivered prehardened to 240-270 HB.The surface of the steel can be flame-hardened without water cooling to a hardness of 58±2..
Tensile Strength, Yield 670 MPa

@Strain 0.200 %
97200 psi

@Strain 0.200 %
Bisalloy Steels BisPlate 70 Thickness >80-100 mm
Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness. Can be welded with minimal preheat and has excellent low temperat..
Tensile Strength, Yield 670 MPa

@Strain 0.200 %
97200 psi

@Strain 0.200 %
Bisalloy Steels BisPlate 70 Thickness 16-80 mm
Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness. Can be welded with minimal preheat and has excellent low temperat..
Tensile Strength, Yield 670 MPa

@Strain 0.200 %
97200 psi

@Strain 0.200 %
Bisalloy Steels BisPlate 70 Thickness 5 -
Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness. Can be welded with minimal preheat and has excellent low temperat..