Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 65.2 MPa @Strain 0.200 % |
9460 psi @Strain 0.200 % |
|
Malvern Minerals Epoxy with 50% Novacite® Daper Quartz Filler Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |