Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 6.515 MPa | 944.9 psi | |
Microcell Composite Company CELLOMER® 2100 SBS Rubber Pellets CELLOMER® PELLETS can be used in hot-pressing or with injection foaming boards. Featuring anti-slippage and elasticity.Information provided by Microcell Composite Company |