Polymer Property : Tensile Strength, Yield = 93500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 645 MPa

@Strain 0.200 %,
Temperature 760 °C
93500 psi

@Strain 0.200 %,
Temperature 1400 °F
Haynes 214® alloy, cold rolled annealed sheet 2.0-3.2 mm thick
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Yield 645 MPa

@Strain 0.200 %
93500 psi

@Strain 0.200 %
Haynes 556® alloy, 10% cold reduction
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..