Mechanical Properties Metric English Comments
Tensile Strength, Yield 6.4077 MPa
929.36 psi
-7% change after 70 hours @ 225°C; ASTM D412
Precision Polymer Engineering S75R Silicone Rubber
Oil Resistant, Red Silicone Rubber, 65-75 °IRHD. Diesel Liner Ring Grade. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applic..