Tensile Strength, Yield 638 MPa

@Strain 0.200 %
92500 psi

@Strain 0.200 %
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 15.9 mm thick bar
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Tensile Strength, Yield 638 MPa

@Strain 0.200 %
92500 psi

@Strain 0.200 %
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 15.9 mm thick plate, aged 3 hours at 816°C
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..