Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 920 MPa | 133000 psi | |
Industeel Superplast® SP300 Prehardened Mold Steel Superplast® 300 (SP300) is a prehardened steel with a BHN 300 (32 HRC) to be used for plastic injection molds, extrusion dies, and compression molds offering improved performance for the mold mak.. |
|||
Tensile Strength, Yield | 920 MPa @Strain 0.200 % |
133000 psi @Strain 0.200 % |
|
Haynes 230® alloy, 20% cold reduction Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Tensile Strength, Yield | >= 920 MPa | >= 133000 psi | 50<x=60mm |
ThyssenKrupp XABO® 960 Structural Steel This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli.. |
|||
Tensile Strength, Yield | 920 MPa @Temperature 23.0 °C |
133000 psi @Temperature 73.4 °F |
0º, Conditioning: 23°C; ASTM D3039 |
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Woven Carbon Prepreg 42% resin weight with C193PW(HTA) - 193 g/m2 plain weave 3K HTA 49% fiber volumeInformation provided by HexCel |