Polymer Property : Tensile Strength, Yield = 9140 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 - 63.0 MPa

@Temperature -40.0 - 80.0 °C
2760 - 9140 psi

@Temperature -40.0 - 176 °F
Average value: 41.0 MPa Grade Count:2
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..