Mechanical Properties Metric English Comments
Tensile Strength, Yield 903.9 MPa

@Strain 0.200 %
131100 psi

@Strain 0.200 %
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 24% Cold Work
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 24% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m..