Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 9.20 MPa | 1330 psi | ASTM D412 |
Vicone High Performance Rubber VicoSilâ„¢ 909E-BK High Performance Silicone Rubber Information provided by Vicone |
|||
Tensile Strength, Yield | 9.20 MPa | 1330 psi | |
Dow LDPE 955I Low Density Polyethylene DOW LDPE 955I resin is a medium molecular weight distribution homo polymer designed to offer excellent clarity and flexibility, and good toughness, with low warpage. Typical applications include lid.. |
|||
Tensile Strength, Yield | 9.20 MPa @Strain 300 % |
1330 psi @Strain 300 % |
ASTM D412 |
Dow SE BR-1220L Stereospecific high cis-1,4 Polybutadiene (BR) SE BR-1220L is manufactured by a solution process using cobalt catalyst which produces polymers with a very light color and low ash content. A non-staining stabilizer is added during the production.. |