Polymer Property : Tensile Strength, Yield = 9.114 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 9.114 MPa
1322 psi
108% Retention; Air Over Aged 1008 hrs at 100°C, Parallel
Teknor Apex TEKRON® 4300-D88A Thermoplastic Elastomer
Information provided by Teknor Apex Company