Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 885 MPa @Strain 0.200 %, Temperature 650 °C |
128000 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes 25 alloy, cold worked sheet, 20% cold reduction, aged at 370°C (700°F) for 1 hour Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | 885 MPa @Strain 0.200 % |
128000 psi @Strain 0.200 % |
Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of rod; more specific form/thickness entries are also available in MatWeb.Industry Specifications: USA Aeros.. |