Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 850 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 850 - 1050 MPa
123000 - 152000 psi
Swaged after Sintering
MarkeTech 95-3-2 Tungsten Alloy, AMS-T-21014 Class 3
Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st..
Tensile Strength, Yield 850 MPa

@Strain 0.200 %
123000 psi

@Strain 0.200 %
Precipitation Hardened. Value at room temperature
Special Metals INCONEL® Alloy X-750
A nickel-chromium alloy similar to INCONEL alloy 600 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good resistance to corrosion and oxidation along with hig..
Tensile Strength, Yield 850 MPa

@Strain 0.200 %
123000 psi

@Strain 0.200 %
Precipitation Hardened. Value at room temperature
Special Metals NIMONIC® Alloy 115
A precipitation-hardenable nickel-chromium-cobalt alloy with an addition of molybdenum for solid-solution strengthening. It is similar to NIMONIC alloy 105 but has higher levels of aluminum and tit..
Tensile Strength, Yield >= 850 MPa
>= 123000 psi
After bake hardening
SSAB Tunnplat Docol® 1000 DP High-strength Steel
High-strength SteelCharacteristics: The steels are annealed at temperatures between 750°C and 850°C, depending on the grade of steel, and then are hardened by quenching in water. Tempering is..
Tensile Strength, Yield >= 850 MPa
>= 123000 psi
80<x=100mm
ThyssenKrupp XABO® 960 Structural Steel
This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli..
Tensile Strength, Yield 850 MPa
123000 psi
90º, RT, Dry; EN2561
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 50%/G939 HS Carbon
Information provided by HexCel
Tensile Strength, Yield 850 MPa

@Strain 0.200 %
123000 psi

@Strain 0.200 %
Haynes 25 alloy, room temperature after 10% cold reduction
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall..
Copyright © lookpolymers.com All Rights Reserved