Mechanical Properties Metric English Comments
Tensile Strength, Yield 5.85 MPa
848 psi
200%, post cured- 8 hours at 166°C; ASTM D412
Multibase SILASTIC® 7-6860 Dow-Corning Biomedical Grade Liquid Silicone Rubber
Information provided by Multibase