Mechanical Properties Metric English Comments
Tensile Strength, Yield 57.23 MPa
8301 psi
2 in per min; ASTM D638
Network Polymers MS 200 Styrene Methyl Methacrylate Copolymer
Description: Styrene Methyl Methacrylate CopolymerInformation provided by Network Polymers Inc.