Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 572 MPa @Diameter 12.7 mm |
83000 psi @Diameter 0.500 in |
|
Kaiser 7068 T76, T76511 Rod & Bar Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig.. |
|||
Tensile Strength, Yield | 572 - 669 MPa | 83000 - 97000 psi | 0.2% offset |
Eagle Brass 725 Copper Nickel Tin, Spring Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |