Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 5.70 MPa | 827 psi | ASTM D412 |
Polymax® Maxelast® C4940 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Strength, Yield | 5.70 MPa | 827 psi | ASTM D412 |
Precision Polymer Engineering S65A Silicone Rubber Low Compression Set, Blue Silicone Rubber, 65-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Low compre.. |
|||
Tensile Strength, Yield | 5.70 MPa | 827 psi | ASTM D412 |
Precision Polymer Engineering S65B Silicone Rubber Low Compression Set, Black Silicone Rubber, 65-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Low compr.. |
|||
Tensile Strength, Yield | 5.70 MPa | 827 psi | ASTM D412 |
Precision Polymer Engineering S65G Silicone Rubber Low Compression Set, Green Silicone Rubber, 65-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Low compr.. |
|||
Tensile Strength, Yield | 5.70 MPa | 827 psi | ASTM D412 |
Precision Polymer Engineering S65W Silicone Rubber Low Compression Set, Off-white Silicone Rubber, 65-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Low c.. |
|||
Tensile Strength, Yield | 5.70 MPa | 827 psi | ASTM D412 |
Precision Polymer Engineering S65Z Silicone Rubber Low Compression Set, Grey Silicone Rubber, 65-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Low compre.. |