Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 826 MPa @Strain 0.200 % |
120000 psi @Strain 0.200 % |
Typical, Transverse Direction |
Industeel CLC 1.2738 Prehardened Mold Steel (300HB/30HRC) for Thick Sections Description: CLC 1.2738 is a 300HB (30HRC) pre-hardened grade specially designed for plastic mold industry. Chromium, Molybdenum, Nickel carbon and manganese additions are optimized to have a fully .. |