Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 5.625 MPa | 815.8 psi | -25% change after 70 hours @ 200°C; ASTM D412 |
Precision Polymer Engineering S80B Silicone Rubber Black Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Excellent heat resistance and .. |
|||
Tensile Strength, Yield | 5.625 MPa | 815.8 psi | -25% change after 70 hours @ 200°C; ASTM D412 |
Precision Polymer Engineering S80G Silicone Rubber Green Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Excellent heat resistance and .. |
|||
Tensile Strength, Yield | 5.625 MPa | 815.8 psi | -25% change after 70 hours @ 200°C; ASTM D412 |
Precision Polymer Engineering S80Y Silicone Rubber Yellow Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Excellent heat resistance and.. |
|||
Tensile Strength, Yield | 5.625 MPa | 815.8 psi | -25% change after 70 hours @ 200°C; ASTM D412 |
Precision Polymer Engineering S80Z Silicone Rubber Grey Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Excellent heat resistance and l.. |