Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 810 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 810 MPa

@Strain 0.200 %,
Temperature 425 °C
117000 psi

@Strain 0.200 %,
Temperature 797 °F
Haynes 242® alloy, cold rolled sheet, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Tensile Strength, Yield 810 MPa

@Strain 0.200 %
117000 psi

@Strain 0.200 %
Haynes 625 alloy, plate after 8000 hours at 650°C (1200°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Tensile Strength, Yield 810 MPa

@Strain 0.200 %
117000 psi

@Strain 0.200 %
Precipitation Hardened. Value at room temperature
Special Metals INCOLOY® Alloy 925
A precipitation-hardenable nickel-iron-chromium alloy with additions of molybdenum and copper. It combines the high strength of a precipitation-hardenable alloy with the excellent corrosion resista..
Copyright © lookpolymers.com All Rights Reserved