Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 807 MPa @Strain 0.200 %, Temperature 538 °C |
117000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Carpenter Thermo-Span® Fe-Co-Ni Superalloy Data provided by Carpenter Technology Corporation.Thermo-Span® alloy is a precipitation hardenable superalloy which exhibits a low coefficient of thermal expansion over a broad temperature range, h.. |