Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 8.5974 MPa | 1246.9 psi | -3.4% change after 70 hours @ 100°C; ASTM D412 |
Precision Polymer Engineering J70P Butyl Rubber Phenolic/Resin cured Butyl Rubber, 65-75 IRHD. Isobutylene-Isoprene Rubber.Applications: Butyl is resistant to the same fluids as Ethylene Propylene (EPDM). It has excellent resistance to gas permea.. |