Polymer Property : Tensile Strength, Yield = 8.046 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 8.046 MPa
1167 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 5725 Fluorocarbon-Elastomer
Formulated Viton®. General service.Information provided by Seals Eastern, Inc.