Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.00 - 8.00 MPa | 580 - 1160 psi | Average value: 5.67 MPa Grade Count:3 |
Overview of materials for Very Low Density Polyethylene (VLDPE) This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va.. |