Tensile Strength, Yield 54.99 MPa
7975 psi
2 in/min; ASTM D638
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene
DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman.
Tensile Strength, Yield 54.99 MPa
7975 psi
2 in/min; ASTM D638
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene
DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman.
Tensile Strength, Yield 54.99 MPa
7975 psi
2 in/min; ASTM D638
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene
DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman.
Tensile Strength, Yield 54.99 MPa
7975 psi
2 in/min; ASTM D638
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene
DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman.
Tensile Strength, Yield 54.99 MPa
7975 psi
2 in/min; ASTM D638
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene
DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman.
Tensile Strength, Yield 54.99 MPa
7975 psi
2 in/min; ASTM D638
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene
DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman.
Tensile Strength, Yield 54.99 MPa
7975 psi
ASTM D638, DIN EN ISO 527
Ensinger Tecaform™ SAN Polyacetal (POM)
TECAFORM™ (Polyacetal) and TECAPRO™ SAN (Polypropylene), provide an additional safety factor in reducing incidence of bacterial contamination. The raw materials are charged with an antimicrobial ..