Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 54.9 MPa | 7960 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers DIAMALOY 761 ABS/PC Alloy, Non-Halogen Flame Retardant with 5% PTFE Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |