Mechanical Properties Metric English Comments
Tensile Strength, Yield 54.23 MPa
7866 psi
chs 2 in/min; ASTM D638
Diamond Polymers ASA/PC TA-35
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.