Polymer Property : Tensile Strength, Yield = 7850 psi
Polymer Property :
Tensile Strength, Yield =
7850 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
54.1
MPa
7850
psi
ASTM D638
Spartech Royalite R922 PC/ABS Aircraft Grade Sheet
Description: Aircraft Grade SheetInformation provided by Spartech.