Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 53.5 MPa @Temperature 23.0 °C |
7760 psi @Temperature 73.4 °F |
ASTM D638 |
PolyOne Geon™ CPVC EC050 Polyvinyl Chloride, Chlorinated (CPVC) The Geon EC050 CPVC is an extrusion compound for Industrial Pipe applications where enhanced resistance at elevated temperatures is needed. Geon EC050 demonstrates ease of processing and excellent t.. |
|||
Tensile Strength, Yield | 53.5 MPa @Temperature 23.0 °C |
7760 psi @Temperature 73.4 °F |
ASTM D638 |
PolyOne Geon™ CPVC EC950 Polyvinyl Chloride, Chlorinated (CPVC) The Geon EC950 CPVC is an extrusion compound for Industrial Pipe applications where enhanced resistance at elevated temperatures is needed. It is listed under NSF Std 14 and 61. Geon EC950 demonstra.. |