Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 775 MPa | 112000 psi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 20% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |