Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 529 MPa @Strain 0.200 % |
76700 psi @Strain 0.200 % |
|
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 40% Cold Work Tensile strength (ultimate and yield), elongation, and reduction of area values are for annealed then cold worked samples. This produces ASTM grain size 10.0. Other property values are typical of .. |