Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 76.32 MPa | 11070 psi | ASTM D638 |
Omni Plastics OmniTuff™ CPP GRC43 Copolymer Polypropylene Glass Reinforced Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni.. |