Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 340 - 520 MPa | 49300 - 75400 psi | |
Materion Beryllium Copper Alloy 10 Rod and Bar; H (TD04) Temper; up to 76 mm (UNS C17500) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 370 - 520 MPa | 53700 - 75400 psi | |
Materion Beryllium Copper Alloy 10 Wire; H (TD04) Temper; 1.3-12.7 mm Diameter (UNS C17500) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 340 - 520 MPa | 49300 - 75400 psi | |
Materion Beryllium Copper Alloy 3 Rod and Bar; H (TD04) Temper; up to 76 mm (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 420 - 520 MPa | 60900 - 75400 psi | |
ArcelorMittal HSLA 420 High strength low alloy steel for cold forming, Cold Rolled Available in the following: uncoated (HC420LA), electroglavanized (HC420LA +ZE) and Extragal®/galfan/Galvannealed (HC420LA+Z/+ZA/+ZF)Description: Steels in the HSLA (High Strength Low Alloy) range .. |
|||
Tensile Strength, Yield | 340 - 520 MPa | 49300 - 75400 psi | |
Materion Beryllium Copper Alloy 3 Tube; H (TD04) Temper; up to 76 mm o.d. (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 370 - 520 MPa | 53700 - 75400 psi | |
Materion Beryllium Copper Alloy 3 Wire; H (TD04) Temper; 1.3-12.7 mm Diameter (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |