Polymer Property : Tensile Strength, Yield = 7538 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.98 MPa

@Thickness 3.20 mm
7538 psi

@Thickness 0.126 in
Type 1, 5 mm/min; ASTM D-638
Bhansali Engineering Abstron IMC-45 ABS-PC Alloy
ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali
Tensile Strength, Yield 51.98 MPa

@Thickness 3.20 mm
7538 psi

@Thickness 0.126 in
Type 1, 5 mm/min; ASTM D-638
Bhansali Engineering Abstron IMC-45 ABS-PC Alloy
ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali