Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 746 MPa @Strain 0.200 % |
108000 psi @Strain 0.200 % |
|
Kennametal Stellite Stellite® 6K 12.7 or 22.2 mm plate 13.3 mm^3 volume loss--abrasive wear data. Applications include agitators, augers, ball mills, banbury mills, cams, crusher bearings, dryers, dry presses, dump cars, fans, filters, food machinery, g.. |
|||
Tensile Strength, Yield | 746 MPa @Strain 0.200 %, Temperature 538 °C |
108000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F) Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |